| 1. | For the nitrogen - implanted samples , the initiation of crack is greatly delayed , and crack spacing interval is small . the samples prepared by pecvd and piii technologies have been investigated using homemade gas permeation tester . the excellent barrier 而注入件相对沉积件而言,由于没有明显的界面层,而表现为改性层裂纹间距小,但没有完全开裂,具有优良的耐失效性能。 |